Wooden log home facade restoration.
Bleaching, staining and sealing gaps.
Products used in restoration process
Wood whitener (bleach) STAFOR WHITE
Product intended for the cleaning and bleaching of wood surfaces. Cleans wood from mold, blue fungue and whitening old wood which lost the original color of the surface. After processing the wood will be clean of dark spots and renew natural color.
APPLICATION: Must be applied with brush or spray. Aplication with spray - from a distance of 10 - 15 cm, aplication with brush - by direction of the wood fibers, and must be left to dry for about 30 minutes, after drying wash with water. If necessary, treting can be repeated after 2 hours. Do not mechanically remove mold or alges, it can lead to a dangerous dispute of infection on clean wood. Do not use the product with other whiteners, it can cause the release of dangerous gas - chlorine. Do not use on metal surfaces. Tools should be cleaned with water.
CONSUMPTION: Depending on the type and degree of wood infection, approximately 1l for 4-8 square meters.
APPLICATION: Must be applied with brush or spray. Aplication with spray - from a distance of 10 - 15 cm, aplication with brush - by direction of the wood fibers, and must be left to dry for about 30 minutes, after drying wash with water. If necessary, treting can be repeated after 2 hours. Do not mechanically remove mold or alges, it can lead to a dangerous dispute of infection on clean wood. Do not use the product with other whiteners, it can cause the release of dangerous gas - chlorine. Do not use on metal surfaces. Tools should be cleaned with water.
CONSUMPTION: Depending on the type and degree of wood infection, approximately 1l for 4-8 square meters.
Sealant LOG HOME
Sealant is intended for sealing joints and cracks between the beams of log houses, as well as for sealing other wooden structures. Sealant can be perfectly combined with the wood and has good adhesion and high elasticity. Consolidated sealant is especially non-freezing, ensuring excellent hermetic qualities for wooden buildings in summer and winter. Environmentally impeccable material based on natural linseed oil, it does not contain organic solvents or other hazardous substances. Consolidated sealant can be painted with any kind of paint.
APPLICATION: Apply sealant on a dry and clean surface of beam joint by a special syringe or spatula. Before drying, the surface of the applied sealant must be formed with a spatula moistened in soapy water, making a smooth surface, as well as necessary joint profile. Before sealing, it is recommended to prime wooden surfaces with the linseed oil primer "Gulbuve". Under normal circumstances, a waterproof membrane is formed on a surface of sealant within 4-6 hours, complete drying occurs within 24 hours. Sealing is not recommended below +5 º C, as well as when it is raining.
CONSUMPTION: 160m-180m with one10l (15kg) pail if seam width is app. 1cm. Consumption depends on the application method, on width and depth of the joint.
CONSUMPTION: 160m-180m with one10l (15kg) pail if seam width is app. 1cm. Consumption depends on the application method, on width and depth of the joint.
Linseed oil paint-stain NATURA
Ecological glazing paint - stain on linseed oil base containing best quality mineral pigments. It is suitable for painting of beams, log homes, facades of wooden buildings, wooden panels, furniture, floors and other wooden products. Can be used for all types of wood, outdoor and indoor. The paint deeply soaks into the wood, increase resistance of wood, forms a long-lasting weather and UV resistant paint layer, protecting the wood against moisture and damage. At the same time the paint is permeable for air and water vapor, thus allowing the painted wood to „breathe”.
APPLICATION: The paint should be thoroughly mixed prior and during its application. Poorly soaking wood is recommended to be previously treated by fine sandpaper. The paint shall be applied in thick layer with paintbrush, sponge or paint roll. After 2-4 hours excess not-soaked paint - stain should be removed with cloth. Soaking time depends on wood type and wish able shade of treated wood. It is recommended to apply 2 to 3 paint layers of which each next one should be laid after drying of the previous layer. Formation of a more covering, non-transparent painting will require application of thicker layer and less intense remove of excess paint.
CONSUMPTION: Depends on wood type and condition, average consumption 1l/5-12sq.meters. When treating well-polished wood you should meet 1l/10-12sq.meters, for hand crafted logs 1l/5-6sq.meters.
APPLICATION: The paint should be thoroughly mixed prior and during its application. Poorly soaking wood is recommended to be previously treated by fine sandpaper. The paint shall be applied in thick layer with paintbrush, sponge or paint roll. After 2-4 hours excess not-soaked paint - stain should be removed with cloth. Soaking time depends on wood type and wish able shade of treated wood. It is recommended to apply 2 to 3 paint layers of which each next one should be laid after drying of the previous layer. Formation of a more covering, non-transparent painting will require application of thicker layer and less intense remove of excess paint.
CONSUMPTION: Depends on wood type and condition, average consumption 1l/5-12sq.meters. When treating well-polished wood you should meet 1l/10-12sq.meters, for hand crafted logs 1l/5-6sq.meters.